CP-10 is organic modified bentonite clay. It can be used in low to medium polarity systems.
Typical properties
CompositionOrganic derivative of a montmorillonite clay
AppearanceFine white powder
Moisture content (105 Degree,2hr)Max. 3.5%
Viscosity, mPa.s2000-5000
Loss on ignition, %(1000 Degree)32-35
Bulk density0.46-0.48
Fineness (200 mesh)Min. 98%
Application:
l Paint
l Inks
l Sealant
l Adhesive
Using:
It can be added directly in powder.
Add polar activator and pre-gel procedure can have better performance.
The addition is recommended to be before grinding procedure to get the best effectiveness.
Adding level is commonly 0.2%~1.0%.